Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 345 MPa | 50000 psi | |
Pacific Sintered Materials FN-262-T High Strength Nickel Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability.Equivalent MPIF Specification: FN-0405-45All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | |
Pacific Sintered Materials FX-227-T Infiltrated Steel Powdered Metal Machines and plates well. Good in hydraulic applications. Moderate tolerance control.Equivalent MPIF Specification: FX-1005-50All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | |
PSM Industries Pacific Sintered Metals Infiltrated Steel FX-227-T Powdered Metal Machines and plates well, Good in hydraulic applications, Moderate tolerance control Equivalent MPIF Specifications: FX-1005-50Information Provided by Pacific Sintered Metals, a division of PSM Ind.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | |
PSM Industries Pacific Sintered Metals High Strength Nickel Steel FN-262-T Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability Equivalent MPIF Specification: FN-0405-45Information Provided by Pacific Sintered Metals, a division.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
|
FloMet Fe-3% Si Soft Magnetic Alloy FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | |
Materion BrushBronze® 630 (AMS 4640) 3.0" - 5.0" Information supplied by Brush Wellman Engineered Materials.BrushBronze™ 630 is an Aluminum-Nickel-Bronze alloy that combines high strength along with resistance to wear under severe loading con.. |
|||
Tensile Strength, Yield | 345 - 414 MPa @Strain 0.200 % |
50000 - 60000 psi @Strain 0.200 % |
|
Materion BrushCAST® 275CT Fine Grain Casting Alloy (As Cast) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Tensile Strength, Yield | 345 MPa @Diameter 12.7 mm |
50000 psi @Diameter 0.500 in |
|
Kaiser 6040 T9 Rod & Bar 6040 is a lead-free alternative to 6262. The alloy offers very good machinability along with good corrosion resistance. It also has excellent coating acceptance (anodize response). It can be used in.. |
|||
Tensile Strength, Yield | >= 345 MPa | >= 50000 psi | 0.2% proof |
Kobe Steel KSG12 Titanium alloy with low alloying elements, ASTM Gr. 12, Annealed Nominal Composition: Ti-0.3 Mo-0.8 Ni Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant. Information provid.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 %, Temperature 260 °C |
50000 psi @Strain 0.200 %, Temperature 500 °F |
|
Haynes Hastelloy® G-30® alloy, all-weld metal, GMAW weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
Sheet |
Special Metals INCONEL® HX Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Tensile Strength, Yield | >= 345 MPa | >= 50000 psi | 0.2% offset |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, 3/4 Hard 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |
|||
Tensile Strength, Yield | 345 - 427 MPa | 50000 - 62000 psi | 0.2% offset |
Eagle Brass 19210 XP-10 Copper Iron, 3/4 Hard 19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | Typical |
Dura-Bar 65-45-12 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Tensile Strength, Yield | 345 - 372 MPa @Strain 0.200 %, Thickness 1.02 mm |
50000 - 54000 psi @Strain 0.200 %, Thickness 0.0402 in |
|
AK Steel 11 Cr-Cb™ Ferritic Stainless steel AK Steel 11 Cr-Cb™ has increased silicon levels and is dual stabilized with titanium and columbium. Designed for use in automotive exhaust tubing and other high-temperature applications, this is a.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
|
Carpenter Chrome Core® 18-FM Solenoid Quality Stainless Steel, Stress Relieved Data provided by Carpenter Technology Corporation.This is a soft ferritic material designed for operation in more corrosive environments than tolerated by 18% Cr-Fe Type 430 stainless. This new mat.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | Semi-Processed |
AK Steel DI-MAX® M-43 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | In rolling direction |
AK Steel TRAN-COR® H-0 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | In rolling direction |
AK Steel TRAN-COR® H-2 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Tensile Strength, Yield | >= 345 MPa | >= 50000 psi | |
AK Steel ZINCGRIP® FORMABLE 50K / ASTM A1008 class 1 / SAE J1392 050 XLK, Grade 50 Electrogalvanized Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
Tensile Strength, Yield | 345 - 517 MPa @Strain 0.200 % |
50000 - 75000 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899A 1/2 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
Typical; Annealed Plate |
ATI Allegheny Ludlum AL 22™ Nickel-Base Alloy, UNS N06022 AL 22 alloy is a Ni-Cr-Mo alloy that provides outstanding resistance to pitting, crevice corrosion, intergranular attack, and stress corrosion cracking. The combination of Cr, Ni, Mo, and W provide.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AL 444™ Ferritic Stainless Steel Low carbon, low nitrogen ferritic stainless steel alloy. Characteristics:practically immune to chloride stress corrosion cracking, enhanced resistance to pitting and crevicing, good general corrosi.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
|
ATI Allvac® AL 6XN® UNS N08367 Specialty Steel Uses: Process equipment, flue-gas scrubber systems, multi-effect evaporators for brines, seawater, pulp & paper liquors.Property values are for samples in the metallurgical condition: 2050°F anneal.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® C 22 UNS N06022 Nickel Superalloy Uses: Pressure vessels, pumps, valves, HX tubing and piping for the CPI and HPI. Trays, flanges, fasteners, wire, screens.Property values are for samples in the metallurgical condition: 2050°F age... |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Grade 16 Titanium (UNS R52402) Uses: CPI equipment, industrial components, condenser tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Grade 2 Titanium (UNS R50400) Uses: CPI equipment, industrial components, condenser tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AL 17-7™ High Strength Stainless Steel, UNS S17700 Property data below is typical of annealed samples. Available in sheet and strip. For use in high-strength springs, bellows, and aerospace applications.Information provided by Allegheny Ludlum |
|||
Tensile Strength, Yield | >= 345 MPa | >= 50000 psi | |
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; A (A) Temper; All Sizes (UNS N03360) Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Grade 7 Titanium (UNS R52400) Uses: CPI equipment, industrial components, tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |