Polymer Property : Tensile Strength, Yield = 780 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 780 MPa

@Strain 0.200 %
113000 psi

@Strain 0.200 %
Precipitation Hardened. Value at room temperature
Special Metals NIMONIC® Alloy 80A
A nickel-chromium alloy similar to NIMONIC alloy 75 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good corrosion and oxidation resistance and high tensile a..
Tensile Strength, Yield 780 MPa
113000 psi
SSAB Tunnplat Domex® Wear Steel Sheet
Domex® Wear is a new grade of steel sheet in the Domex® range, and its main distinguishing features are good wear resistance, high strength, good bendability, high toughness and good weldabili..
Tensile Strength, Yield 780 MPa

@Strain 0.200 %
113000 psi

@Strain 0.200 %
Typical
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al), Anneal Strip/Sheet
High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess..
Tensile Strength, Yield 780 MPa

@Strain 0.200 %
113000 psi

@Strain 0.200 %
Haynes 242® alloy, hot rolled plate, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good thermal..
Tensile Strength, Yield 780 MPa

@Strain 0.200 %
113000 psi

@Strain 0.200 %
Haynes 556® alloy, 20% cold reduction
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Yield 780 MPa

@Strain 0.200 %
113000 psi

@Strain 0.200 %
Haynes 625 alloy, 10% cold reduction
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..