SSAB Tunnplat Domex® Wear Steel Sheet

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel
Manufacturer SSAB Tunnplat AB
Trade Name Domex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SSAB Tunnplat Domex® Wear Steel Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Domex® Wear is a new grade of steel sheet in the Domex® range, and its main distinguishing features are good wear resistance, high strength, good bendability, high toughness and good weldability. The wear resistance of Domex® Wear is close to that of much harder quenching and tempering steels.Uses: For components subjected to moderate abrasive wear caused by hard particles, such as stones, sand, ore or slurries. In the building industry: concrete mixers, hoppers. In the transport industry: truck platforms, tippers, sludge conveyors, refuse collection trucks. In agriculture: plough shares, seed conveyors. In the mining industry: fans, screws conveyors.Data provided by SSAB Tunnplat.
Physical Properties Metric English Comments
Density 7.87 g/cc
0.284 lb/in³
Estimated by MatWeb
Mechanical Properties Metric English Comments
Hardness, Brinell 265
265
Tensile Strength, Ultimate >= 800 MPa
>= 116000 psi
Tensile Strength, Yield 780 MPa
113000 psi
Elongation at Break 15 %
15 %
A<sub>5</sub>
Impact 34
34
J/cm²; -20°C; longitudinal
Bend Radius, Minimum >= 2.0 t
>= 2.0 t
Component Elements Properties Metric English Comments
Aluminum, Al 0.040 %
0.040 %
Carbon, C 0.17 %
0.17 %
Chromium, Cr 0.30 %
0.30 %
Iron, Fe 97.14 %
97.14 %
As Remainder
Manganese, Mn 1.8 %
1.8 %
Molybdenum, Mo 0.10 %
0.10 %
Phosphorous, P 0.010 %
0.010 %
Silicon, Si 0.30 %
0.30 %
Sulfur, S <= 0.010 %
<= 0.010 %
Titanium, Ti 0.14 %
0.14 %