Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 53.9 MPa | 7820 psi | ASTM D638 |
Samyang Triloy® 410 PC/PET alloy
(discontinued **) Characteristics:Impact resistantHeat resistantDimensional stabilityProcessabilityGood flowApplications:O/A partRear view mirror housingRice cooker baseAll information provided by Samyang |
|||
Tensile Strength, Yield | 53.9 MPa | 7820 psi | ASTM D638 |
Samyang Triloy® 410N PC/PET alloy, Flame Retardant
(discontinued **) Characteristics:Impact resistantHeat resistantDimensional stabilityProcessabilityFlame retardantApplications:O/A partRear view mirror housingRice cooker baseAll information provided by Samyang |
|||
Tensile Strength, Yield | 53.9 MPa @Thickness 3.20 mm |
7820 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUCEL HI510 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0Information provided by LG Chemical |
|||
Tensile Strength, Yield | 53.9 MPa @Thickness 3.20 mm |
7820 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID HI5001AH PA6/PO, High Melt Strength, High Barrier property, CaCl2 Resistance Feature: Injection Molding, PA6/PO, High Melt Strength, High Barrier property, CaCl2 ResistanceApplication: Automotive (Fuel System Tube)CAS No. 25038-54-4, 9010-79-1 and 9002-88-4Information provid.. |
|||
Tensile Strength, Yield | 53.9 MPa @Thickness 3.20 mm |
7820 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUMIPLAS LD590 Light diffusion ABS Description: Injection Molding, Light diffusion, Medium ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical |
|||
Tensile Strength, Yield | 53.9 MPa @Thickness 3.20 mm |
7820 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUPOL HI2202B PP+GF20%, High Impact Description: Injection Molding, PP+GF20%, General Purpose, High ImpactApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 65997-17-3 and 9010-79-1Information provided by LG Chemica.. |
|||
Tensile Strength, Yield | 53.9 MPa @Thickness 3.20 mm |
7820 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY GP5008BF FR PC/ABS, Flame Retardance, Heat Resistance Description: Injection Molding, PC/ABS, Flame Retardance, Heat ResistanceApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chemical |
|||
Tensile Strength, Yield | 53.9 MPa @Thickness 3.20 mm |
7820 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY HR5007AE PC/ABS, High Impact Description: Injection Molding, PC/ABS, High Flow, High ImpactApplication: E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 53.9 MPa @Thickness 3.20 mm |
7820 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY RF3208F PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2 and 13463-67-1Information provided by LG .. |
|||
Tensile Strength, Yield | 53.9 MPa | 7820 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HI-1001BP PC/ABS, Metal Plating Grade PC/ABS material for platingInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 53.9 MPa | 7820 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HP-1000H PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 53.9 MPa | 7820 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HP-1000XA PC/ABS, Unreinforced PC/ABS material for automobile IP-coreInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 53.9 MPa | 7820 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® NH-0927 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 53.9 MPa | 7820 psi | ASTM D638 |
Samsung Cheil Industries Starex® SF-0505H MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 53.9 MPa | 7820 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GP-5000 PBT, Unreinforced General PBT material that can be used for connectorsInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 53.9 MPa | 7820 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HI-1001BP PC/ABS, Metal Plating Grade PC/ABS material for platingInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 53.9 MPa | 7820 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HN-3104 PC, 10% Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 53.9 MPa | 7820 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HP-1000H PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 53.9 MPa | 7820 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® NH-0927 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 53.9 MPa | 7820 psi | ASTM D638 |
Samsung Cheil Industries Starex® SF-0505H MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 53.9 MPa | 7820 psi | ASTM D638 |
Samyang Triloy® 225 PC/ABS alloy Characteristics:Impact resistantHeat resistantDimensional stabilityApplications:Air con. grillAll information provided by Samyang |
|||
Tensile Strength, Yield | 53.9 MPa | 7820 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GP-5000 PBT, Unreinforced General PBT material that can be used for connectorsInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 53.9 MPa | 7820 psi | ASTM D638 |
Cheng Yu Plastic ML848 Flame Retardant PC |
|||
Tensile Strength, Yield | 53.9 MPa | 7820 psi | ASTM D638 |
Cheng Yu Plastic PP237G2 Polypropylene, 20% Glass Fiber |
|||
Tensile Strength, Yield | 53.9 MPa @Thickness 3.20 mm |
7820 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron IMC-45M ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |
|||
Tensile Strength, Yield | 53.9 MPa | 7820 psi | ASTM D638 |
Cheng Yu Plastic B600 PC/PBT |
|||
Tensile Strength, Yield | 53.9 MPa @Thickness 3.20 mm |
7820 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron IMC-45M ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |
|||
Tensile Strength, Yield | 53.9 MPa | 7820 psi | ASTM D638 |
Cheng Yu Plastic ML1010 PC/PTFE |