Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 786 MPa @Temperature 21.1 °C |
114000 psi @Temperature 70.0 °F |
0° Direction, Dry; Vacuum/Oven Cured; ASTM D3039-95 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 12K BW Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Tensile Strength, Yield | 786 MPa | 114000 psi | After ageing at 70°C / 95% RH; RT |
Hexcel® HexPly® 922-1/35%/G926 180°C Curing Epoxy Matrix 5H satin/370g/m2 carbon fabric: FVC=60%Information provided by HexCel |