Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.52 MPa | 801 psi | cured 60 mins @ 150°C |
ACC QLE 1039 QSI Quantum Silicones 40 Durometer Addition Cure Elastomer for Coating QLE 1039 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: .. |
|||
Tensile Strength, Yield | 5.52 MPa | 801 psi | cured |
ACC QLE 1101 QSI Quantum Silicones Specialty Silicone Coating QLE 1101 is a low viscosity, two-component, addition cure, silicone elastomer.Key Features: Fast cure at elevated temperaturesLow linear shrinkageTransparent, ideal for pigmentationLow viscosity Par.. |