Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ACC QLE 1101 QSI Quantum Silicones Specialty Silicone Coating

Category Polymer , Thermoset , Silicone
Manufacturer Amber Chemical Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC QLE 1101 QSI Quantum Silicones Specialty Silicone Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QLE 1101 is a low viscosity, two-component, addition cure, silicone elastomer.Key Features: Fast cure at elevated temperaturesLow linear shrinkageTransparent, ideal for pigmentationLow viscosity Part of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
"B" component
1.02 g/cc
1.02 g/cc
"A" component
Viscosity 2000 cP
2000 cP
"B" component
2000 cP
2000 cP
"A" component
Storage Temperature <= 38.0 °C
<= 100 °F
12 months
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
cured
Tensile Strength, Yield 5.52 MPa
801 psi
cured
Elongation at Break 300 %
300 %
cured
Thermal Properties Metric English Comments
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
cured
Maximum Service Temperature, Air 204 °C
399 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Optical Properties Metric English Comments
Refractive Index 1.40
1.40
cured
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Cure Time 10.00000 min

@Temperature 150 °C
0.1666667 hour

@Temperature 302 °F
30.0 min

@Temperature 100 °C
0.500 hour

@Temperature 212 °F
Descriptive Properties Value Comments
Color Transparent
"A" component
Transparent
"B" component
Work Life 180 mins
Users viewing this material also viewed the following: