Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 84.1 MPa | 12200 psi | ASTM D638 |
Nilit Polynil® P240HSLV High Viscosity, Heat Stabilized Nylon 66 Description: Polynil P240 HSLV was developed for injection molding applications, where a combination of heat aging resistance, abrasion resistance and impact strength is needed, such as chain tensio.. |
|||
Tensile Strength, Yield | 84.1 MPa | 12200 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ AT-15CF/5T Acetal-Copolymer, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **)&l Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 84.1 MPa | 12200 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/6 GF14 IM HS L 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Tensile Strength, Yield | 84.1 MPa | 12200 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/6 GF14 IM L 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedUL File Nu.. |
|||
Tensile Strength, Yield | 84.1 MPa | 12200 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/6 GF15 IM HS L 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Tensile Strength, Yield | 84.1 MPa | 12200 psi | ASTM D638 |
Techmer ES Electrablend® PA6/6 03002 A MB Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement/Unspecified Filler/Reinfor.Additive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Elec.. |
|||
Tensile Strength, Yield | 84.1 MPa | 12200 psi | ASTM 638 |
PlastxWorld CEVIAN® B5523 15% GF PBT/ABS Alloy Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |