Mechanical Properties Metric English Comments
Tensile Strength, Yield 580 MPa

@Strain 0.200 %
84100 psi

@Strain 0.200 %
Hogen HM1150 Tungsten-Based Metal
Mil Spec T-21014D Class 2; AMS T-21014 Class 2; ASTM B-777-99 Class 2. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE..
Tensile Strength, Yield 580 MPa

@Strain 0.200 %
84100 psi

@Strain 0.200 %
Mi-Tech Metals HD17.5 Tungsten-Based Metal
Mil Spec T-21014D Class 2; AMS T-21014 Class 2; ASTM B-777-99 Class 2; ASTM B-777-07 Class 2. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal con..
Tensile Strength, Yield >= 580 MPa

@Strain 1.00 %
>= 84100 psi

@Strain 1.00 %
Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness
Description: Soleil C5 is a 13% Cr 4 Ni 0.5 Mo martensitic stainless steel. Its nickel content, associated with low carbon ensures better weldability, ductility, impact resistance and fatigue resist..
Tensile Strength, Yield 580 MPa

@Strain 0.200 %
84100 psi

@Strain 0.200 %
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Tensile Strength, Yield 580 MPa

@Strain 0.200 %
84100 psi

@Strain 0.200 %
Bisalloy Steels BisPlate 60 Thickness 5 -
Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness.Applications: Storage Tanks, High Rise Buildings, Lifting Equipment..
Tensile Strength, Yield 580 MPa

@Strain 0.200 %
84100 psi

@Strain 0.200 %
Bisalloy Steels BisPlate 60 Thickness >80-100 mm
Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness.Applications: Storage Tanks, High Rise Buildings, Lifting Equipment..
Tensile Strength, Yield 580 MPa

@Strain 0.200 %
84100 psi

@Strain 0.200 %
Bisalloy Steels BisPlate 60 Thickness 16-80 mm
Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness.Applications: Storage Tanks, High Rise Buildings, Lifting Equipment..
Tensile Strength, Yield 580 MPa
84100 psi
Latrobe Nitralloy® 135 Modified VAC-ARC, 3 to 5 in Premium Nitriding Steel
NITRALLOY 135 MODIFIED VAC-ARC steel is a low alloy nitriding grade with moderate hardenability. It has been designed to provide a high case hardness and to maintain its core strength during the nit..