Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness

Category Metal , Ferrous Metal , Martensitic , Stainless Steel , T S40000 Series Stainless Steel
Manufacturer Groupe Arcelor
Trade Name SOLEIL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Soleil C5 is a 13% Cr 4 Ni 0.5 Mo martensitic stainless steel. Its nickel content, associated with low carbon ensures better weldability, ductility, impact resistance and fatigue resistance properties when compared to 13 Cr ferritic-martensitic grades (AISI 410-420/Euronorms 1.4000 X6 Cr 13). The alloy has good corrosion resistance to fresh water and performs well under erosion-corrosion phenomena. The alloy is specially designed for all applications requiring high mechanical properties combined with high toughness and may be used in medium corrosive conditions. Typical applications are shafts or compressor impellers, particularly for hydraulic applications.Information provided by manufacturer.
Physical Properties Metric English Comments
Density 7.70 g/cc
0.278 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 220 - 320
220 - 320
Typical
Tensile Strength, Ultimate 750 - 950 MPa
109000 - 138000 psi
Minimum Guaranteed
Tensile Strength, Yield >= 560 MPa
>= 81200 psi
Minimum Guaranteed
>= 580 MPa

@Strain 1.00 %
>= 84100 psi

@Strain 1.00 %
Elongation at Break >= 18 %
>= 18 %
Modulus of Elasticity 206 GPa
29900 ksi
Poissons Ratio 0.288
0.288
Calculated
Shear Modulus 80.0 GPa

@Temperature 20.0 °C
11600 ksi

@Temperature 68.0 °F
Charpy Impact >= 80.0 J
>= 59.0 ft-lb
100 J
73.8 ft-lb
Typical
>= 60.0 J

@Temperature 0.000 °C
>= 44.3 ft-lb

@Temperature 32.0 °F
80.0 J

@Temperature 0.000 °C
59.0 ft-lb

@Temperature 32.0 °F
Typical
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 0.000 - 100 °C
6.11 µin/in-°F

@Temperature 32.0 - 212 °F
12.0 µm/m-°C

@Temperature 0.000 - 400 °C
6.67 µin/in-°F

@Temperature 32.0 - 752 °F
Specific Heat Capacity 0.460 J/g-°C

@Temperature 20.0 °C
0.110 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 26.0 W/m-K

@Temperature 20.0 °C
180 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Component Elements Properties Metric English Comments
Carbon, C 0.040 %
0.040 %
Chromium, Cr 13 %
13 %
Iron, Fe 82.039 %
82.039 %
As remainder
Molybdenum, Mo 0.50 %
0.50 %
Nickel, Ni 4.0 %
4.0 %
Phosphorous, P 0.020 %
0.020 %
Silicon, Si 0.40 %
0.40 %
Sulfur, S 0.0010 %
0.0010 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000800 ohm-cm

@Temperature 20.0 °C
0.0000800 ohm-cm

@Temperature 68.0 °F