Polymer Property : Tensile Strength, Yield = 86.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 86.9 MPa
12600 psi
ASTM D638
Omni Plastics OmniTech™ PA6/6,6 V0 125 Flame Retardant
OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and ..
Tensile Strength, Yield 86.9 MPa
12600 psi
ASTM D638
Omni Plastics OmniTech™ PC GR20 Glass Reinforced Polycarbonate
OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and ..
Tensile Strength, Yield 86.9 MPa
12600 psi
ASTM D638
Nilit Polynil® P50FIL Super Fast Cycling, Nucleated Nylon 66
Description: Polynil P50 FIL is a nucleated, internally lubricated NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass produc..
Tensile Strength, Yield 86.9 MPa
12600 psi
ASTM D638
Techmer ES HiFill® PA6 CM40 HS 40% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: Natural ..
Tensile Strength, Yield 86.9 MPa
12600 psi
ASTM D638
Techmer ES HiFill® PA6/6 CM40 6122 BK 40% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackProcessing Method: Injection Mol..
Tensile Strength, Yield 86.9 MPa
12600 psi
ASTM D638
Clariant Renol PP1100G40 Polypropylene Homopolymer, 40% Glass Fiber, Chemically Coupled
Data provided by Clariant Masterbatches