Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 86.9 MPa | 12600 psi | ASTM D638 |
Omni Plastics OmniTech™ PA6/6,6 V0 125 Flame Retardant OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
Tensile Strength, Yield | 86.9 MPa | 12600 psi | ASTM D638 |
Omni Plastics OmniTech™ PC GR20 Glass Reinforced Polycarbonate OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
Tensile Strength, Yield | 86.9 MPa | 12600 psi | ASTM D638 |
Nilit Polynil® P50FIL Super Fast Cycling, Nucleated Nylon 66 Description: Polynil P50 FIL is a nucleated, internally lubricated NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass produc.. |
|||
Tensile Strength, Yield | 87.0 MPa @Strain 0.200 %, Temperature 980 °C |
12600 psi @Strain 0.200 %, Temperature 1800 °F |
|
Haynes 263® alloy, cold rolled sheet, solution treated and aged Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle.. |
|||
Tensile Strength, Yield | 87.0 MPa | 12600 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP GFL36L PSU (Asia Pacific) LNP* Lubricomp* GFL36L is a compound based on Polysulfone resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Tensile Strength, Yield | 87.0 MPa | 12600 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer LNP* LUBRICOMP* KCL34A is a compound based on Acetal Homopolymer resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Tensile Strength, Yield | 87.0 MPa | 12600 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer (Asia Pacific) LNP* Lubricomp* KCL34A is a compound based on Acetal Homopolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive. |
|||
Tensile Strength, Yield | 87.0 MPa | 12600 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP LX82803 PEEK (Europe-Africa-Middle East) LNP* LUBRICOMP* LX82803 is a compound based on Polyetheretherketone resin containing Proprietary Lubricant. Added features include : Internally Lubricated. |
|||
Tensile Strength, Yield | 87.0 MPa | 12600 psi | Type 1A, 50 mm/min; ISO 527-2 |
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK) AvaSpire® AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. .. |
|||
Tensile Strength, Yield | 86.9 MPa | 12600 psi | ASTM D638 |
Techmer ES HiFill® PA6 CM40 HS 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: Natural .. |
|||
Tensile Strength, Yield | 86.9 MPa | 12600 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 CM40 6122 BK 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackProcessing Method: Injection Mol.. |
|||
Tensile Strength, Yield | 87.0 MPa | 12600 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX8408 PPE+PA Noryl GTX* GTX8408 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is glass filled and suitable for injection molding. The elongation of this material is higher than GTX8410W.. |
|||
Tensile Strength, Yield | 87.0 MPa | 12600 psi | ASTM-D638 |
Polyram RamSter PF329G4 PBT, 20% Glass Fiber, Flame Retardant 20% Glass fiber reinforced, halogen free flame retardant PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 87.0 MPa | 12600 psi | dry; ISO 527-1/-2 |
DSM Novamid® 1010C2 PA6 Easy Molding Grade |
|||
Tensile Strength, Yield | 86.9 MPa | 12600 psi | ASTM D638 |
Clariant Renol PP1100G40 Polypropylene Homopolymer, 40% Glass Fiber, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 87.0 MPa | 12600 psi | ISO 527 |
Azoty Tarnow™ TARNOFORM 300 GF3 POM 15% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Tensile Strength, Yield | >= 86.7 MPa | >= 12600 psi | 130 N/25mm; Testing Results |
CEN® Electronic Material CS Polyimide Tape CEN® CS polyimide tape is made of CEN® CN polyimide film coated with a high performance silicone adhesive. The tape shows excellent dielectric and insulation properties, high heat resistant, excel.. |
|||
Tensile Strength, Yield | 87.0 MPa | 12600 psi | ISO 527-2/1A/50 |
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. The .. |
|||
Tensile Strength, Yield | 87.0 MPa | 12600 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East) VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin. |
|||
Tensile Strength, Yield | 87.0 MPa @Strain 0.200 %, Temperature 1093 °C |
12600 psi @Strain 0.200 %, Temperature 1999 °F |
|
Haynes 230® alloy, as cast vacuum investment casting Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Tensile Strength, Yield | 87.0 MPa | 12600 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP GFL36L PSU LNP* Lubricomp* GFL36L is a compound based on Polysulfone resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Tensile Strength, Yield | 87.0 MPa | 12600 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP 2X04505 ETFE LNP* THERMOCOMP* 2X04505 is a compound based on ETFE resin containing Proprietary Filler(s). |
|||
Tensile Strength, Yield | 87.0 MPa | 12600 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP 2X04505 ETFE LNP* THERMOCOMP* 2X04505 is a compound based on ETFE resin containing Proprietary Filler(s). |
|||
Tensile Strength, Yield | 87.0 MPa | 12600 psi | SABIC - Japan Method |
SABIC Innovative Plastics Valox® VSR4150 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |