Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 59.3 MPa | 8600 psi | chs 2 in/min; ASTM D638 |
Network Polymers SAN 300 Natural Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 59.3 MPa | 8600 psi | ASTM D638 |
Polymer Resources PC/ABS-FRG5 Flame Retardant PC/ABS Alloy, 5% Glass Reinforced PC/ABS Alloy, Flame Retardant, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Tensile Strength, Yield | 59.3 MPa | 8600 psi | ASTM D638 |
Ravago Manufacturing Americas Hybrid S466 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 59.3 MPa | 8600 psi | ASTM D638 |
PTS POM-270 27.0 MFI Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 59.3 MPa | 8600 psi | ASTM D638 |
PTS POM-90 9.0 MFI Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 59.3 MPa @Thickness 3.17 mm |
8600 psi @Thickness 0.125 in |
|
KEP Kepital® F20-52 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 59.3 MPa | 8600 psi | ASTM D638 |
Spartech Polycast Solarcryl (0.187") Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Tensile Strength, Yield | 59.3 MPa | 8600 psi | ASTM D638 |
Techmer ES Statiblend® ABS GF20 AS 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 59.3 MPa | 8600 psi | ASTM D638 |
Techmer ES Electrablend® PA6/6 05002 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 59.3 MPa | 8600 psi | ASTM D638 |
Westlake Plastics Pomalux® CN-SS Acetal Copolymer (conductive) Stainless-steel-fiber-filled, non-sloughing, dimensionally stable material HDT @ 264 psi of 225F. This material has relatively high chemical resistance, is extremely strong and stiff, and is an exc.. |
|||
Tensile Strength, Yield | 59.3 MPa | 8600 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers NPP 808 C5 TDS Polycarbonate Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 59.3 MPa | 8600 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers SAN 300 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |