Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 60.4 MPa | 8760 psi | |
Hexcel® HexPly® F593 Epoxy Resin HexPly® F593 is a modified 350°F (177°C) curing epoxy system with very low flow for carbon fabric and tape applications that provides excellent laminate and honeycomb sandwich properties. As a lo.. |