Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 60.7 MPa | 8800 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PC-000/10T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® AT-1000 Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® XT XT-100-BU01-HF Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Tensile Strength, Yield | 60.7 - 68.0 MPa | 8800 - 9860 psi | Average value: 64.6 MPa Grade Count:4 |
Overview of materials for Acrylic, High Flow, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app.. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Fiberfil® J-62/30/E8 Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Techmer ES Luriblend® PP GF20 CC GL2 BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Graphite Powder Lubricant(2%)Features: Chemically Coupled and LubricatedAppearance: BlackInf.. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Techmer ES Plastiblend® POM CO UV BK Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: CopolymerAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Styron EMERGEâ„¢ 4630-10 Polycarbonate EMERGEâ„¢ PC 4630-10 advanced resin is formulated to supply both excellent ultraviolet stability and enhanced ignition resistance while maintaining excellent physical properties and processabilit.. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Techmer ES HiFill® HDPE LGF50 12 mm 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Westlake Plastics Pomalux® Acetal Copolymer Pomalux is a high performance acetal copolymer that has excellent mechanical, electrical, and wear properties. It is engineered to provide outstanding dimensional stability, even when machining par.. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Clariant Renol PCSP0006 Polycarbonate, Laser Markable Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Ensinger Tecaform™ Acetal Copolymer - Extruded Products (POM) Tecaform™ is a semi-crystalline thermoplastic offering high strength, stiffness and toughness. It is resistant to hot water, hydrocarbons and solvents, and it posses good bearing and wear properti.. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Ensinger Tecaform™ FG Blue Food Grade Acetal (POM) Tecaform™ is resistant to hot water and typical cleaning chemicals. It possesses good bearing and wear properties. The blue color makes it more visible than standard grades. It is commonly used .. |