Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 60.7 - 68.0 MPa | 8800 - 9860 psi | Average value: 64.6 MPa Grade Count:4 |
Overview of materials for Acrylic, High Flow, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app.. |
|||
Tensile Strength, Yield | 40.0 - 68.0 MPa @Temperature 60.0 - 140 °C |
5800 - 9860 psi @Temperature 140 - 284 °F |
Average value: 55.3 MPa Grade Count:1 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Tensile Strength, Yield | 63.0 - 68.0 MPa | 9140 - 9860 psi | ASTM D638 |
3D Systems Accura® 55 Plastic for SLA® Systems Simulate the properties and appearance of molded ABS. For use with solid-state stereolithography (SLA®) systems.ApplicationsAutomotive interior componentsShort-run production partsElectronic compon.. |
|||
Tensile Strength, Yield | 66.0 - 68.0 MPa | 9570 - 9860 psi | ASTM D638 |
3D Systems Accura® Bluestone™ Plastic for SLA® Systems A high stiffness engineered nanocomposite that opens new applications for stereolithography users. For use with solid-state stereolithography (SLA®) systems.ApplicationsWind-tunnel testing for the .. |
|||
Tensile Strength, Yield | 58.0 - 68.0 MPa | 8410 - 9860 psi | ASTM D638 |
3D Systems Accura® 60 Plastic for SLA® Systems Simulate the properties and appearance of polycarbonate. For use with solid-state stereolithography (SLA®) systems.ApplicationsTough functional prototypesAutomotive design componentsConsumer electr.. |