Polymer Property : Tensile Strength, Yield = 8900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 57.2 - 61.4 MPa
8300 - 8900 psi
ASTM D638
Alcoa KAMA 4223 Impact Modified RPET  (discontinued **)
CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 50”Silicone coatingCl..