Mechanical Properties Metric English Comments
Tensile Strength, Yield 57.2 MPa
8300 psi
ASTM D638
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant
Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided..
Tensile Strength, Yield 57.2 MPa
8300 psi
ASTM D638
Polymer Resources TP-FR2-[color]-WR Polybutylene Terephthalate, Flame Retardant, Wear Resistant
Polybutylene Terephthalate, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Tensile Strength, Yield 57.2 MPa
8300 psi
ASTM D638
Ravago Manufacturing Americas Hybrid S464 ABS + Polycarbonate Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Tensile Strength, Yield 57.2 MPa
8300 psi
ASTM D638
PTS Trimid® N66-T100HL Toughened, Heat Stabilized, Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 57.2 MPa
8300 psi
ASTM D638
Ravago Manufacturing Americas Hybrid B2035I Polycarbonate + PBT Alloy
Available in North America High Impact Resistance Form: PelletsInformation provided by Ravago
Tensile Strength, Yield 57.2 MPa
8300 psi
2.0 in/min; ASTM D638
LTL Color Compounds ColorFast® PAHF Polycarbonate-ABS Alloy
General purpose HB-rated PC/ABS with improved chemical resistanceAll information provided by LTL Color Compounders, Inc.
Tensile Strength, Yield 57.2 MPa
8300 psi
ASTM D638
Star Plastics PC/PET7901 Molding Grade PC/PET
Information provided by Star Plastics, Inc.
Tensile Strength, Yield 57.2 MPa
8300 psi
ASTM D638
Star Plastics PC20NBR Molding Grade PC with Release
Information provided by Star Plastics, Inc.
Tensile Strength, Yield 57.2 MPa
8300 psi
ASTM D638
Techmer ES HiFill® PC R GY143
Availability: North AmericaForms: PelletsFeatures: Low Smoke EmissionInformation provided by TP Composites, Inc.
Tensile Strength, Yield 57.2 MPa
8300 psi
ASTM D638
Clariant Renol BR7039 Nylon 6 Alloy, bondable to TPU
Data provided by Clariant Masterbatches
Tensile Strength, Yield 57.2 - 61.4 MPa
8300 - 8900 psi
ASTM D638
Alcoa KAMA 4223 Impact Modified RPET  (discontinued **)
CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 50”Silicone coatingCl..
Tensile Strength, Yield 57.2 - 85.0 MPa
8300 - 12300 psi
Average value: 68.7 MPa Grade Count:4
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA)
This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max..