Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.60 MPa
1390 psi
-20% change after 70 hours @ 125°C; ASTM D412
Precision Polymer Engineering E80V Ethylene Propylene Rubber
Peroxide cured, blue-violet coloured Ethylene Propylene Terpolymer, 75-85 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Specially formulated for sealing applications involving high..
Tensile Strength, Yield 9.60 MPa
1390 psi
ASTM D638
DuPont 20 Series 2020 Specialty Polyethylene Resin  (discontinued **)
DuPont 2020T and 2020 specialty low density polyethylene resins are products characterized by low melt index and intermediate crystallinity. These products, produced via a unique polymerization proc..
Tensile Strength, Yield 9.60 MPa
1390 psi
ASTM D638
DuPont 20 Series 2010 Specialty Polyethylene Resin
DuPont 2010 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding fl..
Tensile Strength, Yield 9.60 MPa
1390 psi
ASTM D638
DuPont 20 Series 2020T Specialty Polyethylene Resin
DuPont 2020T and 2020 specialty low density polyethylene resins are products characterized by low melt index and intermediate crystallinity. These products, produced via a unique polymerization proc..
Tensile Strength, Yield 9.60 MPa
1390 psi
ASTM D638
DuPont 20 Series 20-6064 Specialty Polyethylene Resin
DuPont 20-6064 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding..
Tensile Strength, Yield 9.60 MPa
1390 psi
ASTM D638
DuPont 20 Series DPE 20 Specialty Polyethylene Resin
DuPont 20 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding flex..
Tensile Strength, Yield 9.60 MPa

@Treatment Temp. 200 °C,
Time 252000 sec
1390 psi

@Treatment Temp. 392 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Vicone High Performance Rubber VicoSil™ C240Q-RD High Performance Silicone Rubber
Information provided by Vicone
Tensile Strength, Yield 9.60 MPa
1390 psi
Dow DOWLEX™ 2505 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2505 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with good rigidity. It has ex..
Tensile Strength, Yield 9.60 MPa

@Strain 50.0 %
1390 psi

@Strain 50.0 %
Covestro Texin® 250 Urethane Thermoplastic Elastomer
Key Features:UnfilledSuitable processing methods:Injection moldingProfile extrusionSheet extrusionCoatingBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScie..