DuPont 20 Series 2020T Specialty Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name 20 Series
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont 20 Series 2020T Specialty Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuPont 2020T and 2020 specialty low density polyethylene resins are products characterized by low melt index and intermediate crystallinity. These products, produced via a unique polymerization process, have a well earned reputation for processability and outstanding flexibility and environmental stress crack resistance. DPE 2020T and 2020 are identical products with DPE 2020T passing a "tube defect" specification that is not required for DPE2020.Typical Applications: Extruded squeeze tubes for personal care, cosmetic, and pharmaceutical applications; Tube shoulders providing headers for LDPE, HDPE and coextruded squeeze tubes; Low pressure water and air tubing; Rotational molding fittings; Molding of small bottles, caps, seals, etc. for medical, personal care and other applications. Features & Benefits: Superior resistance to environmental stress cracking; High flexibility; Good heat stability; Excellent color; Odor free; Excellent chemical resistance; Tasteless; Nontoxic.Each lot of DPE 2020T passes an internal tube imperfection specification.Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D792
Melt Flow 1.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 51
51
ASTM D2240
Tensile Strength, Ultimate 18.6 MPa
2700 psi
ASTM D638
Tensile Strength, Yield 9.60 MPa
1390 psi
ASTM D638
Elongation at Break 620 %
620 %
ASTM D638
Modulus of Elasticity 0.186 GPa
27.0 ksi
ASTM D638
Flexural Modulus 0.238 GPa
34.5 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
0.430 J/cm

@Temperature -40.0 °C
0.806 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 93.0 °C
199 °F
Freezing Point via DSC/ASTM D3418
109 °C
228 °F
Upon Melting via DSC/ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C
111 °F
ASTM D648
Vicat Softening Point 97.0 °C
207 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746
Optical Properties Metric English Comments
Refractive Index 1.51
1.51
ASTM D542
Processing Properties Metric English Comments
Nozzle Temperature 193 °C
379 °F
Typical die temp for tube extrusion.
Melt Temperature 188 °C
370 °F
tube extrusion