Mechanical Properties Metric English Comments
Tensile Strength, Yield 900 - 1100 MPa
131000 - 160000 psi
Swaged after Sintering
MarkeTech 91-6-3 Tungsten Alloy, AMS-T-21014 Class 1
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st..
Tensile Strength, Yield 900 - 1100 MPa
131000 - 160000 psi
Swaged after Sintering
MarkeTech 92-5-3 Tungsten Alloy, AMS-T-21014 Class 2
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st..
Tensile Strength, Yield 900 - 1100 MPa
131000 - 160000 psi
Swaged after Sintering
MarkeTech 93-4-3 Tungsten Alloy, AMS-T-21014 Class 2
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st..
Tensile Strength, Yield 900 MPa

@Strain 0.200 %
131000 psi

@Strain 0.200 %
Typical
Industeel CREUSABRO® 4000 High Wear Resistant Steel
Description: CREUSABRO® 4000 is a high wear resistant steel, offering a 30 % extra in service life compared to a conventional 400 HB water quenched. Improved properties of CREUSABRO® 4000 resu..
Tensile Strength, Yield 900 MPa
131000 psi
Typical
Industeel CREUSABRO® 4800 Advanced Technology in Wear Steel
Description: CREUSABRO® 4800(P) is a wear resistant steel offering up to 50% extra in service life compared with a 400 HB water quenched steel. CREUSABRO® 4800(P) combines several modern metal..
Tensile Strength, Yield 900 MPa

@Strain 0.200 %,
Temperature 205 °C
131000 psi

@Strain 0.200 %,
Temperature 401 °F
Haynes 242® alloy, cold rolled sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Tensile Strength, Yield 900 MPa

@Strain 0.200 %
131000 psi

@Strain 0.200 %
Typical
TIMET TIMETAL® 685 (Ti-6Al-5Zr-0.5Mo-0.25Si) Titanium Alloy
High-Temperature, High-Strength Creep Resistant AlloyIndustry Specifications: Germany Aerospace: 3.7154. France: T-A6ZD. UK Aerospace Specifications BS TA. 43, 44.Features: TIMETAL 685 possesses ..
Tensile Strength, Yield 900 MPa
131000 psi
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass UD fabric 315 g/m2
Information provided by HexCel
Tensile Strength, Yield 900 MPa
131000 psi
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass UD fabric 430 g/m2
Information provided by HexCel
Tensile Strength, Yield 900 MPa
131000 psi
300% elongation; ASTM D412
Lubrizol Estane® 58070 Thermoplastic Polyurethane
Features: Outstanding resiliency, fuel resistance and low temperature flexibility.Uses: Hose and Tube, Injection Molding, Fabric Coating and Wire/CableAvailable in Americas, Europe, Middle East, Afr..
Tensile Strength, Yield 900 MPa
131000 psi
Hexcel® HexPly® M34 75°C (167°F) Curing Epoxy Matrix, High Strength 12k Carbon Balanced Fabric 600 g/m2
Information provided by HexCel
Tensile Strength, Yield >= 900 MPa

@Strain 0.200 %
>= 131000 psi

@Strain 0.200 %
CLAL-MSX NICLAFOR® 1000 TH3 Quenched/Precipitation Heat Treated, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Tensile Strength, Yield >= 900 MPa

@Strain 0.200 %
>= 131000 psi

@Strain 0.200 %
CLAL-MSX NICLAFOR® 1000 TH4 Quenched/Cold Rolled/Precipitation Heat Treated, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Tensile Strength, Yield 900 MPa

@Temperature 500 °C
131000 psi

@Temperature 932 °F
R<sub>p</sub>02. Short transverse direction.
Assab Steels DIEVAR Hot Work Steel
DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i..
Tensile Strength, Yield 900 MPa

@Temperature 500 °C
131000 psi

@Temperature 932 °F
R<sub>p</sub>02. austenitized 1020°C, tempered 630°C to 48 HRC. Holding time = 30 minutes.
Assab Steels QRO 90 SUPREME Hot Work Steel
QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista..
Tensile Strength, Yield 900 MPa

@Strain 0.200 %
131000 psi

@Strain 0.200 %
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 20% Cold Work
The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co..
Tensile Strength, Yield 900 - 1100 MPa
131000 - 160000 psi
ArcelorMittal Dual Phase 1180 Very high strength steel, Cold Rolled Steel
Description: Dual Phase steels offer an outstanding combination of strength and drawability as a result of their microstructure, in which a hard martensitic or bainitic phase is dispersed in a soft ..
Tensile Strength, Yield 900 MPa
131000 psi
ThyssenKrupp SECURE MS special® Structural Steel
This Material Specification applies to the high-strength thermomechanically rolled special steel SECURE MS special® (ThyssenKrupp security steel for civil use) with a hardness from 350 to 450 HBW a..