Material Notes:
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of steel and are more than 50% heavier than lead. Due to their high density, tungsten alloys offer greater radiation shielding than lead and are non-toxic. Tungsten alloys are electrically and thermal conductive and offer good corrosion resistance. They also have a low coefficient of expansion and have a high modulus of elasticity. Because of these unique properties tungsten alloys are used extensively in military applications, balance weights, aircraft components, nuclear and medical shields, fishing and sport tackle, rocket components, tool vibration dampers, electrical contacts, etc.Applications:Nuclear and medical radiation shielding for x-ray and shields for radiation therapy and industrial applications.Aircraft and helicopter rotor balance weightsInstrument balance weightsWeights for sport equipmentTool damping cutter barsHigh voltage contactsInformation provided by MarkeTech International.
Physical Properties Metric English Comments
Density 17.6 g/cc
0.636 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 26 - 30
26 - 30
Sintered Only
35 - 45
35 - 45
Swaged after Sintering
Tensile Strength, Ultimate 900 - 1100 MPa
131000 - 160000 psi
Sintered Only
1150 - 1250 MPa
167000 - 181000 psi
ASwaged after Sintering
Tensile Strength, Yield 900 - 1100 MPa
131000 - 160000 psi
Swaged after Sintering
Elongation at Break 7.0 - 18 %
7.0 - 18 %
Swaged after Sintering
16 - 24 %
16 - 24 %
Sintered Only
Impact 30
30
J/cm²; Swaged after Sintering
90
90
J/cm²; Sintered Only
Component Elements Properties Metric English Comments
Iron, Fe 3 %
3 %
Nickel, Ni 4 %
4 %
Tungsten, W 93 %
93 %