Polymer Property : Tensile Strength, Yield = 94.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 94.5 MPa
13700 psi
ASTM D638
Solvay Specialty Polymers KetaSpire® KT-810 Polyetheretherketone (PEEK)
KetaSpire® KT-810 is an ultra-high molecular weight natural PEEK resin having a melt viscosity ranging from 0.51-0.65 kPa-s as compared to 0.38-0.50 kPa-s for standard high-viscosity PEEK grades ..
Tensile Strength, Yield 94.5 MPa
13700 psi
ASTM D638
Solvay Specialty Polymers KetaSpire® KT-810FP Polyetheretherketone (PEEK)
KetaSpire® KT-810FP is the fine powder form of KT-810 resin. KT-810 is an ultra-high molecular weight natural PEEK resin having a melt viscosity ranging from 0.51-0.65 kPa-s as compared to 0.38-0..
Tensile Strength, Yield 94.5 MPa
13700 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® ATH-25GF/000 Acetal-Homopolymer, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Yield 94.5 MPa
13700 psi
ASTM 638
PlastxWorld CEVIAN® B2704 20% GF PBT/ABS Alloy
Glass fiber reinforced PBT/ABS alloy.Information provided by PlastxWorld Inc.