Polymer Property : Tensile Strength, Yield = 94000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 648 MPa

@Diameter 12.7 mm
94000 psi

@Diameter 0.500 in
Kaiser 7068 T6, T651 Rod & Bar
Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig..
Tensile Strength, Yield 648 MPa

@Temperature 23.0 °C
94000 psi

@Temperature 73.4 °F
Hexcel® HexPly® 954-2A Curing Cyanate Resin, Quartz Fiber Reinforced 8 Harness Satin Fabric
Information provided by HexCel