Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 952 MPa @Strain 0.200 % |
138000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 482°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Tensile Strength, Yield | 952 MPa @Strain 0.200 % |
138000 psi @Strain 0.200 % |
|
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 746°C (1375°F)/8hr/AC to 621°C (1150°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |