Polymer Property : Tensile Strength, Yield = 9600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 66.2 MPa
9600 psi
ASTM D638
Polymer Resources PC-HH Polycarbonate, High Heat
Polycarbonate, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resource..
Tensile Strength, Yield 66.2 MPa
9600 psi
ASTM D638
Polymer Resources PC-HH-UV Polycarbonate, High Heat, UV-stabilized
Polycarbonate, High Heat, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P..
Tensile Strength, Yield 66.2 MPa
9600 psi
2.0 in/min; ASTM D638
LTL Color Compounds ColorFast® PCGF110 Polycarbonate, 10% Glass-Filled
High modulus 10% glass-filled polycarbonate, V2-rated, general purposeAll information provided by LTL Color Compounders, Inc.
Tensile Strength, Yield 66.2 MPa
9600 psi
ASTM D638
Techmer ES HiFill® TPU GF40 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc.
Tensile Strength, Yield 66.2 MPa
9600 psi
ASTM D638
Washington Penn Homopolymer Polypropylene 20% Glass Reinforced
Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. ..
Tensile Strength, Yield 66.2 MPa
9600 psi
ASTM D638
Westlake Plastics Zelux® 10% GF Polycarbonate 10% Glass Filled
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
Tensile Strength, Yield 66.2 MPa
9600 psi
2.0 in/min; ASTM D638
LTL Color Compounds ColorFast® FRPC310 Polycarbonate, Flame-Retarded
V0-rated 10% glass-filled polycarbonate, excellent impact strengthAll information provided by LTL Color Compounders, Inc.