Mechanical Properties Metric English Comments
Tensile Strength, Yield 67.6 MPa
9800 psi
ASTM D638
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 67.6 MPa
9800 psi
ASTM D638
Polymer Resources AH-GP1-[color]-H Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 67.6 MPa
9800 psi
ASTM D638
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, Heat Stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 67.6 MPa
9800 psi
ASTM D638
Polymer Resources AH-GP2-[color]-H Acetal Homopolymer, Medium Flow, General Purpose Molding, Heat Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 67.6 MPa
9800 psi
ASTM D638
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin, Heat Stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 67.6 MPa
9800 psi
ASTM D638
Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 67.6 - 141 MPa
9800 - 20500 psi
Average value: 98.2 MPa Grade Count:17
Overview of materials for ABS/Polyester Alloy + GF
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro..
Tensile Strength, Yield 67.6 MPa
9800 psi
ASTM D638
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 67.6 MPa
9800 psi
ASTM D638
Global GPP-240C 40% Glass Reinforced, Chemically Coupled Impact Polypropylene
Information provided by Global Polymers Corporation.
Tensile Strength, Yield 67.6 MPa
9800 psi
ASTM D638
Techmer ES Luriblend® HTN 05007
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, High Heat Resistance and LubricatedAppearance: BlackInformation provided by TP Composites, ..
Tensile Strength, Yield 67.6 MPa
9800 psi
ASTM D638
PlastxWorld CEVIAN® EG506 ABS
Inherently Static Dissipative and Glass Fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by Plastx..
Tensile Strength, Yield 67.6 MPa
9800 psi
chs 2 in/min; ASTM D638
Diamond Polymers ABS 3501 GF-20
Description: Reinforced Grade, 20%Glass FilledInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 67.6 MPa
9800 psi
ASTM D638
Asahi Kasei Thermylene® P6-20FG-0753 20% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Tensile Strength, Yield 67.6 MPa
9800 psi
ASTM D638
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength  (Unverified Data**)
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 67.6 MPa
9800 psi
ASTM D638
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, General Purpose Molding  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 67.6 MPa
9800 psi
ASTM 638
PlastxWorld CEVIAN® B5522 10% GF PBT/ABS Alloy
Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc.