Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 67.6 - 141 MPa | 9800 - 20500 psi | Average value: 98.2 MPa Grade Count:17 |
Overview of materials for ABS/Polyester Alloy + GF This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro.. |
|||
Tensile Strength, Yield | 11.7 - 141 MPa | 1700 - 20500 psi | Average value: 42.0 MPa Grade Count:90 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Tensile Strength, Yield | 26.0 - 141 MPa | 3770 - 20500 psi | Average value: 71.0 MPa Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |