Mechanical Properties Metric English Comments
Tensile Strength, Yield 6.83 MPa
990 psi
@ 50% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® 520 Perfluoroelastomer
Chemraz® 520 is recommended for a wide variety of semiconductor equipment dry processing applications where seal reliability with minimal contaminations is required. Additionally, Chemraz 520 of..
Tensile Strength, Yield 6.83 MPa
990 psi
Elastic; ASTM D412
Multibase Multi-Flex® A 7321 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantUV Resistance, Good Processability, Good..
Tensile Strength, Yield 6.83 MPa

@Strain 100 %
990 psi

@Strain 100 %
Saint-Gobain Tygon® S3™ Silver Antimicrobial Tubing
Plasticizer-free inner boreFormulated with a silver based compound on I.D. surfaceO.D. surface can also be formulated with a silver based compoundReduces formulation of biofilm and mildewInhibits gr..
Tensile Strength, Yield 6.83 MPa
990 psi
ASTM D412
Teknor Apex APEX® 3211-50 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling..
Tensile Strength, Yield 6.83 MPa
990 psi
ASTM D412
Teknor Apex Flexalloy® 3501-35-NT Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe..