Polymer Property : Tensile Strength, Yield = 999 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 6.89 MPa
999 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Gravi-Tech™ GRV-PB-069-BMX Natural Polyether Block Amide (PEBA-Ether)
Information provided by PolyOne
Tensile Strength, Yield 6.89 MPa
999 psi
ASTM D412
Precision Polymer Engineering S75R Silicone Rubber
Oil Resistant, Red Silicone Rubber, 65-75 °IRHD. Diesel Liner Ring Grade. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applic..
Tensile Strength, Yield 6.89 MPa
999 psi
200°C for 1,000 hrs
Fujipoly Industries Sarcon® 45H Thin-Film HR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Tensile Strength, Yield 6.89 MPa
999 psi
cured 72 hrs @ RT
ACC QM 262 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material
QM262 is a two component, room temperature, addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin ..