Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 6.89 MPa | 1000 psi | Mixed 1:2; TM R050-36 |
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | TM R050-36 |
Resinlab® EP1285HD-12 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Tensile Strength, Yield | 6.89 MPa | 999 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Gravi-Tech™ GRV-PB-069-BMX Natural Polyether Block Amide (PEBA-Ether) Information provided by PolyOne |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | chs 20 in/min; ASTM D412 |
Network Polymers Softflex® 0826 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | TM R050-36 |
Resinlab® EP1294 Mineral Filled, Flame Retardant Epoxy Syntactic Foam Resinlab™ EP1294 is a two part mineral filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-exti.. |
|||
Tensile Strength, Yield | 6.89 - 13.8 MPa | 1000 - 2000 psi | ASTM D1708 |
Technetics Group Texolon™ 9406 PTFE
(Unverified Data**) General purpose 25% glass filled PTFE for applications less demandingPTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Diel.. |
|||
Tensile Strength, Yield | 6.89 MPa | 999 psi | 200°C for 1,000 hrs |
Fujipoly Industries Sarcon® 45H Thin-Film HR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | @100% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 615 Perfluoroelastomer Greene Tweed’s Chemraz® 615 exhibits outstanding high temperature properties, with a temperature range from 0°F to 615°F (-18°C to 324°C). Chemraz 615’s chemical resistance.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 3005 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowFoamableHeat StabilizedGeneral PurposeOzone ResistantProce.. |
|||
Tensile Strength, Yield | >= 6.89 MPa @Strain 300 % |
>= 1000 psi @Strain 300 % |
|
Sibur SKD 1st Grade Butadiene Rubber (BR) BR 1220. It is used in tires and the rubber and asbestos technical industries. Rubbers produced on a base of butadiene rubber are extremely resistant to wearing. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412-98 |
Saint-Gobain Norprene® A-60-G Industrial Grade Tubing Formulation Description: Norprene® Industrial Grade Tubing, Formulation A-60-G: Norprene® Industrial Grade Tubing outperforms neoprene, EPDM and other general-purpose tubings in test after test and appl.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex APEX® 3210-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2760 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2890M Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | Longitudinal |
Saint-Gobain Norton® Fluorglas® Chemfilm® R128/R129 Premium Grade Extruded Full Density PTFE Film (0.010" thick) Description: Full Density Unsintered Tape is used as primary insulation for high-temperature wires, jackets and cables and wall for convoluted hose. It meets the requirements of component insulation.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex TEKBOND® 6000-45 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | 2 in/min; ASTM D638 |
A. Schulman SCHULAFLEX® SF 302 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF302 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | 2 in/min; ASTM D638 |
A. Schulman SCHULAFLEX® SF 302 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF302 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | |
Tra-Con Tra-Bond 2162D Color Coded Smooth Paste Epoxy Adhesive TRA-BOND 2162D epoxy system is color-coded for easy mixing and handling as a smooth paste, and it develops strong bonds to most materials including metals, glass, ceramics, leather, wood, concrete a.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | 2 in/min; ASTM D638 |
A. Schulman SCHULAFLEX® SF 302 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF302 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | 2 in/min; ASTM D638 |
A. Schulman SCHULAFLEX® SF 302 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF302 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Tensile Strength, Yield | >= 6.89 MPa | >= 1000 psi | ASTM D638 |
Buckeye Polymers BP FLEX 7000 VPL BLK Thermoplastic Elastomer TPV Product Information: BP Flex TPV's are partially vulcanized thermoplastic elastomers designed to meet higher end applications that require the following performance criteria.Product Features:Higher .. |
|||
Tensile Strength, Yield | >= 6.89 MPa | >= 1000 psi | ASTM D638 |
Buckeye Polymers BP FLEX D4107 C BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Tensile Strength, Yield | >= 6.89 MPa | >= 1000 psi | ASTM D638 |
Buckeye Polymers BP FLEX D4107 CU BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Tensile Strength, Yield | 6.89 MPa | 999 psi | cured 72 hrs @ RT |
ACC QM 262 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material QM262 is a two component, room temperature, addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin .. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3201-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® IT 38-096 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerOpaqueApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Extrusion and MoldingPolyOne First ChoiceDisclai.. |
|||
Tensile Strength, Yield | 6.89 - 20.7 MPa | 1000 - 3000 psi | Average value: 16.5 MPa Grade Count:5 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® IT 38-082 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerOver-Molding GradeTransparentMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided b.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | TM R050-36 |
Resinlab® EP1305 Black Highly Toughened Urethane Modified Epoxy Resinlab™ EP1305 Black is a highly toughened urethane modified epoxy designed for bonding PVC, metals, ceramics and other difficult to bond substrates. The system has a thixotropic non-sag viscosi.. |