Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hydrostatic Design Basis | 6.89 MPa @Temperature 60.0 °C |
1000 psi @Temperature 140 °F |
ASTM D2837 |
Total HDPE XT10 N High Density Polyethylene - Pipe Resin Polyethylene: High molecular weight, bimodal pipe resin.Characteristics:Outstanding high temperature creep rupture strengthExceptional slow crack growth resistanceExcellent resistance to rapid crac.. |
|||
Hydrostatic Design Basis | 6.89 MPa @Temperature 60.0 °C |
1000 psi @Temperature 140 °F |
ASTM D2837 |
Total HDPE XT10B High Density Polyethylene, Pipe Resin Polyethylene: HDPE Bimodal PE4710 pipe resin (Black)Characteristics:Outstanding high temperature creep rupture strengthOutstanding slow crack growth resistanceExcellent resistance to rapid crack pr.. |
|||
Hydrostatic Design Basis | 6.89 MPa @Temperature 60.0 °C |
1000 psi @Temperature 140 °F |
ASTM D2837 |
Total HDPE XT25N High Density Polyethylene, Pipe Resin Polyethylene: High molecular weight, bimodal pipe resin. PPI TR4 designation PE4710 /PE100 for demanding installations. Every batch certified to meet 2500 hrs PENT according to ASTM F1473.Charact.. |