Polymer Property : Tensile Modulus = 0.00440 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.00440 GPa
0.638 ksi
Henkel Hysol Benzoxazine 99110 Infusion Resin
One-part Infusion resin for RTM & VARTM processing. Low viscosity, high hot-wet properties and very good resistance against flame, smoke and toxicity.