Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0207 - 0.0345 GPa | 3.00 - 5.00 ksi | TM R050-36 |
Resinlab® EP1295 Black Medium Viscosity, Halogen Free, Flame Retardant Epoxy Casting Resin Resinlab™ EP1295 Black is a medium viscosity, halogen free, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (.. |