Mechanical Properties Metric English Comments
Tensile Modulus 0.0207 - 0.0345 GPa
3.00 - 5.00 ksi
TM R050-36
Resinlab® EP1295 Black Medium Viscosity, Halogen Free, Flame Retardant Epoxy Casting Resin
Resinlab™ EP1295 Black is a medium viscosity, halogen free, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (..
Tensile Modulus 0.0207 GPa
3.00 ksi
ASMT D638 Die C
3M Scotch-Weld™ TE230 Black Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..