Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.240 GPa | 34.8 ksi | ISO 527-1/-2 |
DSM Arnitel® PL471 45 Shore D, Injection Grade Copolyester Elastomer (North America)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.240 GPa | 34.8 ksi | |
LyondellBasell Lupolen® 2452 D SW 413 LDPE Cable sheathingData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.240 GPa | 34.8 ksi | |
LyondellBasell Lupolen® 1852 H SW 413 LDPE Blow moldings, injection moldings.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.240 GPa | 34.8 ksi | |
LyondellBasell Lupolen® 1840 D LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.240 GPa | 34.8 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP PDXF89080 PE LNP* LUBRICOMP* PDXF89080 is a compound based on Polyethylene containing Proprietary Fillers. Added feature of this grade is: Wear Resistant. |
|||
Tensile Modulus | 0.240 GPa | 34.8 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer LNP* LUBRICOMP* YL003 is a compoudn based on Polyester Elastomer resin containing 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Tensile Modulus | 0.240 GPa | 34.8 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP YP003 POLYESTER ELASTOMER LNP LUBRICOMP* YP003 is a compound based on Polyester Elastomer resin containing 15% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 0.240 GPa | 34.8 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp YP003 TPEE LNP LUBRICOMP* YP003 is a compound based on TPEE resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas .. |
|||
Tensile Modulus | 0.240 GPa | 34.8 ksi | ISO 527-1/-2 |
DSM Arnitel® PL460-S 46 Shore D Copolyester Elastomer, Injection Grade (Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.240 GPa | 34.8 ksi | ISO 527-1/-2 |
DSM Arnitel® PL460-S 46 Shore D, Injection Grade, Flame Retardant Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.240 GPa | 34.8 ksi | |
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Tensile Modulus | 0.240 GPa | 34.8 ksi | ISO 527-1/-2 |
DSM Arnitel® PL471 Polyether Ester Elastomer (European Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |