Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 0.335 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.335 GPa
48.6 ksi
ASTM D638
Ashley Polymers Ashlene® 745 Nylon 6/69
A special copolymer ideal for blown and cast film coextrusion. This is a gel free resin with outstanding lot to lot consistency being produced by a continuous process. It has a lower melting point..
Tensile Modulus 0.335 GPa
48.6 ksi
ASTM D638
Ashley Polymers Ashlene® 746 Nylon 6/69
A special copolymer ideal for blown and cast film coextrusion. This is a gel free resin with outstanding lot to lot consistency being produced by a continuous process. It has a lower melting point..