Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.375 GPa | 54.4 ksi | ISO 527-1/-2 |
Quadrant EPP TIVAR® Oil Filled PE-UHMW + oil (ISO Data) TIVAR Oil Filled is a self-lubricating PE-UHMW material in the real meaning of the word. Next to an enhanced wear resistance, the incorporated and evenly dispersed oil renders this material a consid.. |
|||
Tensile Modulus | 0.375 GPa | 54.4 ksi | 1 mm/min |
Arkema Group Rilsan® BMN P40 D Nylon 11 (Conditioned) Designation ISO 1874-PA11-P,MR,12-003Flexible grade for injection molding. Available colors: black, natural and white. Mold release agent.Flexibility. Outstanding working properties. Easy filling of.. |