Tensile Modulus 0.375 GPa
54.4 ksi
ISO 527-1/-2
Quadrant EPP TIVAR® Oil Filled PE-UHMW + oil (ISO Data)
TIVAR Oil Filled is a self-lubricating PE-UHMW material in the real meaning of the word. Next to an enhanced wear resistance, the incorporated and evenly dispersed oil renders this material a consid..
Tensile Modulus 0.375 GPa
54.4 ksi
1 mm/min
Arkema Group Rilsan® BMN P40 D Nylon 11 (Conditioned)
Designation ISO 1874-PA11-P,MR,12-003Flexible grade for injection molding. Available colors: black, natural and white. Mold release agent.Flexibility. Outstanding working properties. Easy filling of..