Mechanical Properties Metric English Comments
Tensile Modulus 0.467 GPa

@Temperature 170 °C
67.7 ksi

@Temperature 338 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Rynite® FR515 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 NC010 is a flame retardant 15% glass reinforced modified polyethylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm..