Polymer Property : Tensile Modulus = 0.480 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.480 GPa

@Temperature 23.0 °C
69.6 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Hytrel® 7246HS BK320 TPC-ET  (Unverified Data**)
Hytrel® 7246HS BK320 is a high modulus, heat stabilized, black grade with nominal hardness of 72D.Information provided by DuPont
Tensile Modulus 0.480 GPa
69.6 ksi
Kuraray HYBRAR® PH2 Polypropylene Blend
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb..
Tensile Modulus 0.480 GPa
69.6 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON MD000IS PP
LNP STAT-KON* MD000IS is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Tensile Modulus 0.480 GPa
69.6 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP (Asia Pacific)
LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Tensile Modulus 0.480 GPa
69.6 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® XE 4180 black 9992 PA1010
Product description: Grilamid XE 4180 black 9992 is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4180 black 9992 is highly ..
Tensile Modulus 0.480 GPa
69.6 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® XE 4180 nat PA1010
Product description: Grilamid XE 4180 natural is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4180 NATURAL is highly resist..
Tensile Modulus 0.480 GPa
69.6 ksi
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 7246HS BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers
Tensile Modulus 0.480 GPa
69.6 ksi
1 mm/min
Arkema Group Rilsan® BESN P20 TL Nylon 11, Flexible Tubing Grade (Conditioned)
Designation ISO 1874-PA11-P,EHL,22-004Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.Flexibility. High impact strength. Very good chemical resistan..
Tensile Modulus 0.480 GPa
69.6 ksi
1 mm/min
Arkema Group Rilsan® BMN P20 D Nylon 11 (Conditioned)
Designation ISO 1874-PA11-P,MR,12-004Flexible grade for injection molding. Available colors: black and natural. Mold release agent.Outstanding working properties. Easy filling of the mold due to its..
Tensile Modulus 0.480 GPa
69.6 ksi
1 mm/min
Arkema Group Kynar® FLEX 2750 PVDF  (discontinued **)
Designation ISO 12086-VDF/HFP-K, EG1NS, M. ?E7.B.F.A.C,, ? (4-10)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousne..
Tensile Modulus 0.480 GPa
69.6 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP
LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Tensile Modulus 0.480 GPa
69.6 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Stat-kon MD000IU PP
LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa..
Tensile Modulus 0.480 GPa
69.6 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Stat-kon MD000IU PP (Asia Pacific)
LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa..