Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 0.500 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.00345 GPa
0.500 ksi
Type IV, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible XV 3716 Polyvinyl Chloride, Flexible (PVC, Flexible)
A Filled PVC compound formulated specifically for FDA extrusion and Molding applications.The physical properties listed below, are typical values obtained on compression molded sheets and tested in ..