Material Notes:
A Filled PVC compound formulated specifically for FDA extrusion and Molding applications.The physical properties listed below, are typical values obtained on compression molded sheets and tested in accordance with accepted test methods. This compound is certified with USP 23 Class 6 requirements when pigmented to Green 1681 and Green 5503 tints.NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high water content only. This statement is only an overview of the FDA listings for this product. It is the customer's responsibility to ensure that the compound is suitable for its intended application.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
10 sec; ASTM D2240
Tensile Strength at Break 10.3 MPa
1490 psi
Type IV, 5.1 mm/min; ASTM D638
Elongation at Yield 350 %
350 %
Type IV, 5.1 mm/min; ASTM D638
Tensile Modulus 0.00345 GPa
0.500 ksi
Type IV, 5.1 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D746
Descriptive Properties Value Comments
Agency Ratings FDA Food Contact, Unspecified Rating
USP XXIII, Class VI
Appearance Light Green
Features Food Contact Acceptable
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America