Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.636 GPa | 92.2 ksi | 1% Secant; 50mm/min; ASTM D638 |
LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 a.. |