Polymer Property : Tensile Modulus = 92.2 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.636 GPa
92.2 ksi
1% Secant; 50mm/min; ASTM D638
LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade
ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 a..