Polymer Property : Tensile Modulus = 0.758 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.621 - 0.758 GPa
90.0 - 110 ksi
ITW Plexus Plexusâ„¢ MA590 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, long open time product and bond lines up to 1" thickInformation provided by Illinois ..