Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | >= 0.900 GPa | >= 131 ksi | 2% sec, MD; ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 6152C (526H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Tensile Modulus | >= 0.900 GPa | >= 131 ksi | 2% sec, MD; ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 4252A (524H1) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-2000 TO Polypropylene Block-Copolymer Based Compound INNOPOL® CS 2-2000 TO is a polypropylene block-copolymer based compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-2000 TO is developed for producing injection m.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 4-8000 Polypropylene Random Copolymer INNOPOL® CS 4-8000 is a polypropylene random copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 4-8000 is highly suitable for pressure pipe manufacturing, includi.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | ISO 527 |
Iran Petrochemical (PCC) BL2 HF 4750 High Density Polyethylene BL2 is a high density polyethylene with 1-Butene as co monomer. It is high impact strength and slightly, lower stiffness than BL3, outstanding resistance to stress cracking, even in contact with su.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | |
Kuraray HYBRAR® PH8 Polypropylene Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | Conditioned; ISO 527-1,-2 |
Lanxess Durethan® B 40 SK 000000 Nylon 6 PA 6, non-reinforced, injection molding |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE (Europe-Africa-Middle East) LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing PTFE. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | ISO 527 Type 1A |
Solvay TECHNYL® B 238 Black 21 N PA66/6, Conditioned Description: Unreinforced and modified copolyamide 66/6, heat stabilized, with improved impact resistance, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 238 is particular.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | 1mm/min; ISO 527 |
Styrolution Styrolux 3G55 SBC Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp TH0450D LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific) LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | ISO 527-2 |
Borealis Borpact™ SG910MO Polypropylene for Injection Molding Borpact™ SG910MO is a high impact and transparent polypropylene. This grade provides high gloss, high transparency and excellent impact properties. Applications: containers and products with medium.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | 1mm/min; ISO 527 |
Borealis RA130E-1498 Polypropylene Random Copolymer RA130E-1498 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is white colored. Applications: RA130E-1498 is recommended for the production of PP-R p.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | 1mm/min; ISO 527 |
Borealis RA130E-6015 Polypropylene Random Copolymer RA130E-6015 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Tensile Modulus | 0.900 GPa @Temperature 100 °C |
131 ksi @Temperature 212 °F |
DIN 53457 |
Zell-Metall Engineering Plastics Zellamid 1100 MO Improved sliding and self lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | 1mm/min; ISO 527-2 |
Borealis RB607MO Polypropylene Random Copolymer RB607MO is a random copolymer for blow molding, with good transparency and contact clarity, very good gloss and surface finish. Bottles up to 2 liters can be steam sterilized due to heat distortion .. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | ISO 527-1, 2 |
Polyplastics Duracon® SX-35 Acetal Co-polymer (POM), Flexible, Lower noise DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BZ 1/2 PA6 Product description: Grilon BZ 1/2 is an unreinforced, impact modified PA6 injection molding grade with normal melt viscosity. Grilon BZ 1/2 has the following important properties: Good flow behavio.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BR 40 PA6 Product description: Grilon BR 40 is a medium viscosity, unreinforced, heat stabilized PA6 grade for injection mounding and extrusion applications. Grilon BR 40 has the following important propertie.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FN727 NC010A Nylon 6
(Unverified Data**) Toughened Polyamide 6Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST801 is an unreinforced super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity r.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | ASTM D638 |
Azdel SuperLite® SL551800-100 PP Resin Matrix / 55% Glass Fiber (10 mm Molded Thickness) AZDEL SuperLite® SL551800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | ASTM D638 |
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (12 mm Molded Thickness) AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | |
BASF Novolen® 2700 L Polypropylene UV stabilized grade for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | |
BASF Novolen® 3200 H Polypropylene Blow moldings and thermoformed parts.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | |
BASF Novolen® 3200 MC Polypropylene Cast film without slip and blocking agents.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-30 MHLS Polyamide 6 - Colored High viscosity heat and UV light stabilized grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP FP003 PE (Europe-Africa-Middle East) LNP *Lubricomp* FP003 is a compound based on Polyethylene resin, containing PTFE and Silicone. Added features include: Internally Lubricated. |