Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.439 GPa @Temperature -20.0 °C |
1514.1 ksi @Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9330 NC010 PBT+SAN
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9330 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |