Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 10.54 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 10.54 GPa
1529 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DEP23FXC PC
LNP STAT-KON* DEP23FXC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 10% PTFE/Silicone. Added features include: Electrically Conductive. Wear Resistant, Superior Molding.
Tensile Modulus 10.54 GPa
1529 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DX06413H PC
LNP* THERMOCOMP* DX06413H is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Tensile Modulus 10.54 GPa
1529 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF006L PA 66
LNP* THERMOCOMP* RF006L is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Low Extractible.
Tensile Modulus 10.54 GPa
1529 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF006L PA 66 (Asia Pacific)
LNP* Thermocomp* RF006L is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Low Extractible.
Tensile Modulus 10.54 GPa
1529 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF006LXP PA 66
LNP* THERMOCOMP* RF006LXP is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Low Extractible.
Tensile Modulus 10.54 GPa
1529 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RX02743 PA 66
LNP* Thermocomp* RX02743 is a compound based on Nylon 66 resin containing Glass Fiber.
Tensile Modulus 10.54 GPa
1529 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RX02743 PA 66 (Asia Pacific)
LNP* Thermocomp* RX02743 is a compound based on Nylon 66 resin containing Glass Fiber.
Tensile Modulus 10.54 GPa
1529 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP UF0067W PPA
LNP* THERMOCOMP* UF0067W is a compound based on Polyphthalamide resin containing 30% glass fiber. Added features of this material include: Hot Water Moldable, Non-Brominated & Non-Chlorinated Flam..
Tensile Modulus 10.54 GPa
1529 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DEP23FXC PC (Asia Pacific)
LNP STAT-KON* DEP23FXC is a compound based on Polycarbonate resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.