Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 11.56 GPa
1677 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Verton RV008ESV_GY7E072 PA 66
Preliminary data for 40% long glass fiber filled, single color pellet gray, PA66This data was supplied by SABIC-IP for the Americas region.